Mechanical Properties Metric English Comments
Tenacity 0.370 - 0.509 N/tex
4.19 - 5.77 g/denier
Average value: 0.447 N/tex Grade Count:3
Overview of materials for Nylon 610
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Tenacity 0.370 N/tex
4.19 g/denier
GB/T14337-2008
Sichuan Deyang Haton® 5.5 dtex Polyphenylene Sulfide Staple Fiber
Excellent chemical stabilityInformation provided by Sichuan Deyang Chemical Co., LTD
Tenacity 0.370 - 0.463 N/tex
4.19 - 5.25 g/denier
EMS-Griltech Grilon® XA 136 Nylon 610 Monofilament (Super-Set)
Description: GRILON XA 136 is a Nylon 610 based monofilament for paper machine, clothing, forming screen, and filtration.Special Note: GRILON Monofilament has been bought by ShakespeareData provid..