Polymer Property : Tenacity = 4.30 g/denier Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tenacity 0.380 N/tex
4.30 g/denier
3.8 lb. load
Shakespeare WonderThread® SN-40 ultra soft TEX# 45 Nylon Industrial Sewing Thread
Used for sewing: Bedspreads, Comforters, Caps, Hats, Blankets, Stuffed Toys, Pillows, Carpets and Rugs, Handbags, Indoor Furniture, Curtains and Drapes, Apparel, Sleeping BagsInformation provided b..
Tenacity 0.380 N/tex
4.30 g/denier
Knot Strength
UBE 5034T Nylon 6/66 Monofilament (Drawing Ratio=5.5)
Specialties: High viscosity Nylon 6/66 Copolymer, Higher transparent and softness than 5033T, High tenacity Applications: Small size sport fishing line and long- line (main line)Information provided..