Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 690 MPa | 100000 psi | |
Arkema Group Orgalloy® LE 60THM Flexible Nylon Alloy (Conditioned) LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).higher in rigidity than LE 6000. For film, hollow vessel blow moldi.. |