Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 1050 MPa | 152000 psi | ISO 899 |
Styrolution Styrolux 656C SBC Styrolux 656C is a high flow thermoplastic injection molding styrene-butadiene block copolymer. It has crystal clarity, good toughness, good stiffness, and warpage resistance for general molding ap.. |
|||
Tensile Creep Modulus, 1000 hours | 1050 MPa | 152000 psi | ISO 899 |
BASF Ultraform N 2640 Z2 UNC Q600 POM Ultraform N2640 Z2 UNC Q600 is an elastomer-modified grade of POM for injection molding with high impact strength. |
|||
Tensile Creep Modulus, 1000 hours | 1050 MPa @Strain <=0.500 % |
152000 psi @Strain <=0.500 % |
ISO 899-1 |
BASF Ultraform® E 3120 BM POM Description: Is a POM, high-molecular grade for extrusion blow molding of hollow parts.Information provided by BASF |