Tensile Creep Modulus, 1000 hours 1050 MPa
152000 psi
ISO 899
Styrolution Styrolux 656C SBC
Styrolux 656C is a high flow thermoplastic injection molding styrene-butadiene block copolymer. It has crystal clarity, good toughness, good stiffness, and warpage resistance for general molding ap..
Tensile Creep Modulus, 1000 hours 1050 MPa
152000 psi
ISO 899
BASF Ultraform N 2640 Z2 UNC Q600 POM
Ultraform N2640 Z2 UNC Q600 is an elastomer-modified grade of POM for injection molding with high impact strength.
Tensile Creep Modulus, 1000 hours 1050 MPa

@Strain <=0.500 %
152000 psi

@Strain <=0.500 %
ISO 899-1
BASF Ultraform® E 3120 BM POM
Description: Is a POM, high-molecular grade for extrusion blow molding of hollow parts.Information provided by BASF