Mechanical Properties Metric English Comments
50% Modulus 0.00500 GPa
0.725 ksi
ISO 527-2/5A/500
Lubrizol Advanced Materials Pearlthane® 11T85 Polycaprolactone Copolyester based TPU
Type : Pearlthane® 11T85 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Adequate hardness, excellent mechanical propert..
50% Modulus 0.00500 GPa
0.725 ksi
ISO 527-2/5A/500
Lubrizol Advanced Materials PEARLTHANE® 11T85E Thermoplastic Polyurethane Elastomer
Type: Pearlthane® 11T85E is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining hardness with excellent mechanical pr..
50% Modulus 0.00500 GPa
0.725 ksi
ISO 527-2/5A/500
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer
Type : Pearlthane® CLEAR 15N85 is a polyether copolymer-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Outstanding colour, a very low yellowness index as..
50% Modulus 0.00500 GPa
0.725 ksi
ISO 527-2/5A/500
Lubrizol Advanced Materials PEARLTHANE® 91T85 Thermoplastic Polyurethane Elastomer
Type : Pearlthane® 91T85 is a aliphatic-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Low density, fast processing and excellent elasticity properties.A..
50% Modulus 0.00500 GPa
0.725 ksi
DIN 53504
Lubrizol ESTANE® T5090 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
50% Modulus 0.00500 GPa
0.725 ksi
ISO 37
Lubrizol ESTANE® GP85AB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 85AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsInformation provided by Lubrizol.
50% Modulus 0.00500 GPa
0.725 ksi
ASTM D412
C.O.I.M. LARIPUR® LPR9060EF PTMG Polyether Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
50% Modulus 0.00500 GPa
0.725 ksi
DIN 53504
Lubrizol ESTANE® 58214 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
50% Modulus 0.00500 GPa
0.725 ksi
DIN 53504
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..