Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.01591 GPa | 2.308 ksi | ASTM D1414, ASTM D412 |
DuPont Performance Polymers Kalrez® AeroSeal™ 7797 Fluoroelastomer DuPont™ Kalrez AeroSeal™ 7797 perfluoroelastomer parts are a specialty black product specifically targeted for use in applications requiring high hardness/higher modulus properties. It offers outs.. |
|||
50% Modulus | 0.01591 GPa | 2.308 ksi | ASTM D1414, ASTM D412 |
DuPont Performance Polymers Kalrez® Spectrum™ 7090 Fluoroelastomer DuPont™ Kalrez Spectrum™ 7090 perfluoroelastomer parts are specifically targeted for use in applications requiring high hardness/higher modulus properties. These specialty black parts have excelle.. |