DuPont Performance Polymers Kalrez® AeroSeal™ 7797 Fluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer DuPont Performance Polymers (Former DuPont Elastomers)
Trade Name Kalrez®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Kalrez® AeroSeal™ 7797 Fluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DuPont™ Kalrez AeroSeal™ 7797 perfluoroelastomer parts are a specialty black product specifically targeted for use in applications requiring high hardness/higher modulus properties. It offers outstanding thermal stability and compression set resistance and has excellent seal force retention properties. It also offers excellent resistance to HTS (High Thermo-Oxidative Stability) gas turbine engine lubricating oils and has excellent response to temperature cycling effects. Kalrez AeroSeal™ 7797 has excellent mechanical properties and is well suited for both static and dynamic sealing applications. A maximum continuous service temperature of 325 C (617 F) is suggested. Short excursions to higher temperatures may also be possible. Performance Features/Benefits Outstanding thermal stability Outstanding compression set resistance Excellent seal force retention properties Excellent resistance to high thermo-oxidative stability (HTS) gas turbine engine lubricating oils Excellent response to temperature cycling effects Excellent mechanical properties Lower coefficient of thermal expansion (CTE) versus other Kalrez® products thus minimizing the need to increase the free volume of the seal gland when upgrading from fluoroelastomers (FKM) to perfluoroelastomers (FFKM).
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ASTM D2240
Tensile Strength at Break 23.84 MPa
3458 psi
ASTM D1414, ASTM D412
Elongation at Break 77 %
77 %
ASTM D1414, ASTM D412
50% Modulus 0.01591 GPa
2.308 ksi
ASTM D1414, ASTM D412
Compression Set 11 %

@Temperature 204 °C,
Time 252000 sec
11 %

@Temperature 399 °F,
Time 70.0 hour
ASTM D1414 and ASTM D395B
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 325 °C
617 °F
DuPont Test Method
Minimum Service Temperature, Air -5.00 °C
23.0 °F
Retraction Temperature, Tr10; ASTM D1329
Descriptive Properties Value Comments
Color Black