Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 117 MPa | 17000 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® 4012 PBT (Europe-Africa-Middle East) VALOX 4012 is a 10% high strength glass fibre reinforced PBT injection moulding resin with improved mechanical properties. Applications: connectors. |
|||
Hardness, H358/30 | 117 MPa | 17000 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® 4012G PBT VALOX 4012G is a 10% glass fiber reinforced PBT injection molding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility. |
|||
Hardness, H358/30 | 117 MPa | 17000 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East) VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin. |