Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 265 MPa | 38400 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® V9561 PET (Europe-Africa-Middle East) Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances. |