Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 65.0 MPa | 9430 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP (Europe-Africa-Middle East) PPX7110 is an alloy of PP and PPO, providing high impact and good heat resistance. Generic identification acc. ISO11469: >PP+PPE+PS-I |