Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Rupture Strength = 45.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Rupture Strength 45.0 MPa

@Temperature 982 °C,
Time 3.60e+6 sec
6530 psi

@Temperature 1800 °F,
Time 1000 hour
2 mm sheet
Haynes NS-163® Cobalt Alloy
Alloy that brings high-temperature alloy performance at temperatures up to 2200°F (1204°C). HAYNES NS-163 alloy is a wrought cobalt-based alloy (Co–28Cr–21Fe–9Ni–1.25Tiâ€..
Rupture Strength 45.0 MPa

@Temperature 925 °C,
Time 36000 sec
6530 psi

@Temperature 1700 °F,
Time 10.0 hour
Initial Stress
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750)
Haynes X-750 (UNS No. N07750) alloy is an age-hardenable, nickel-base superalloy with very good strength at temperatures up to about 1600°F (870°C). It is widely used as a wrought material for..
Rupture Strength 45.0 MPa

@Temperature 800 °C,
Time 3.60e+7 sec
6530 psi

@Temperature 1470 °F,
Time 10000 hour
Stress Rupture
AFE Technologies Cronite 37Ni/18Cr/Nb No. HR32
High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF..
Copyright © lookpolymers.com All Rights Reserved