Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 31.1 J @Thickness 3.20 mm, Temperature 23.0 °C |
22.9 ft-lb @Thickness 0.126 in, Temperature 73.4 °F |
3.39 m/sec, Peak Energy; ASTM D3763 |
Styron MAGNUMâ„¢ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 3325 MT is a resin with excellent processing characteristics and matt surface finish. The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines.. |
|||
Dart Drop, Total Energy | 31.0 J @Temperature 23.0 °C |
22.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
Lubrizol Isoplast® 101LGF40NAT Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Dart Drop, Total Energy | 31.0 J @Temperature 23.0 °C |
22.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
Lubrizol Isoplast® 2540 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Dart Drop, Total Energy | 31.0 J @Temperature 23.0 °C |
22.9 ft-lb @Temperature 73.4 °F |
Total Energy; ASTM D3763 |
Dow T702-12N Polypropylene Impact Copolymer Resin Dow Announced Sale of Global Polypropylene Business to Braskem in July 2011. |
|||
Dart Drop, Total Energy | 31.0 J @Temperature -17.8 °C |
22.9 ft-lb @Temperature 0.000 °F |
ASTM D3763 |
Styron INSPIRE™ TF3800 Polypropylene Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010 |