Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow T702-12N Polypropylene Impact Copolymer Resin

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Dow Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow T702-12N Polypropylene Impact Copolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Index of Compound 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.7 MPa
3000 psi
ISO 527-2/50
Tensile Modulus 1.10 GPa
160 ksi
ISO 527-2
Flexural Modulus 1.15 GPa
167 ksi
ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²

@Temperature -20.0 °C
4.76 ft-lb/in²

@Temperature -4.00 °F
ISO 180
13.0 kJ/m²

@Temperature -10.0 °C
6.19 ft-lb/in²

@Temperature 14.0 °F
ISO 180
48.0 kJ/m²

@Temperature 23.0 °C
22.8 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Dart Drop, Total Energy 20.0 J

@Temperature 23.0 °C
14.8 ft-lb

@Temperature 73.4 °F
Peak Energy; ASTM D3763
31.0 J

@Temperature 23.0 °C
22.9 ft-lb

@Temperature 73.4 °F
Total Energy; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 78.0 °C
172 °F
Unannealed; ISO 75-2/B