Polymer Property : Dart Drop, Total Energy = 29.5 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 40.0 J

@Temperature -30.0 °C
29.5 ft-lb

@Temperature -22.0 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® C1000HF PC+ABS
High flow PC+ABS.
Dart Drop, Total Energy 40.0 J

@Temperature -30.0 °C
29.5 ft-lb

@Temperature -22.0 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® C1000HF PC+ABS (Asia Pacific)
High flow PC+ABS.
Dart Drop, Total Energy 40.0 J

@Temperature -30.0 °C
29.5 ft-lb

@Temperature -22.0 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS
Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.
Dart Drop, Total Energy 40.0 J

@Temperature -30.0 °C
29.5 ft-lb

@Temperature -22.0 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Asia Pacific)
Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.
Dart Drop, Total Energy 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® LG9000 PC+ABS
PC+ABS blend, low gloss and UV-stable, suitable for automotive interior applications.
Dart Drop, Total Energy 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® LG9000 PC+ABS (Asia Pacific)
PC+ABS blend, low gloss and UV-stable, suitable for automotive interior applications.
Dart Drop, Total Energy 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® MC1300 PC+ABS
Cycoloy MC1300 resin is an injection moldable PC/ABS blend with excellent flow and impact performance. It is designed for plating applications mostly used in the automotive industry.
Dart Drop, Total Energy 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® MC1300 PC+ABS (Asia Pacific)
Cycoloy MC1300 resin is an injection moldable PC/ABS blend featuring excellent flow and impact performance. It is designed for plating applications mostly used in automotive industry.
Dart Drop, Total Energy 40.0 J

@Temperature -30.0 °C
29.5 ft-lb

@Temperature -22.0 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® C1110 PC+ABS
High impact and ductility at 73F (23C) and -20F (-29C).
Dart Drop, Total Energy 40.0 J

@Temperature -30.0 °C
29.5 ft-lb

@Temperature -22.0 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® C1110 PC+ABS (Asia Pacific)
High impact and ductility at 73F (23C) and -20F (-29C).
Dart Drop, Total Energy 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics GELOY XTPM405 ASA+PC
High flow PC/ASA with improved impact at room and low temperatures. Improved release. Excellent weatherability for outdoor unpainted or clearcoated applications. Injection Moldable with large color ..