Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 40.0 J @Temperature -30.0 °C |
29.5 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C1000HF PC+ABS High flow PC+ABS. |
|||
Dart Drop, Total Energy | 40.0 J @Temperature -30.0 °C |
29.5 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C1000HF PC+ABS (Asia Pacific) High flow PC+ABS. |
|||
Dart Drop, Total Energy | 40.0 J @Temperature -30.0 °C |
29.5 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Dart Drop, Total Energy | 40.0 J @Temperature -30.0 °C |
29.5 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Asia Pacific) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Dart Drop, Total Energy | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® LG9000 PC+ABS PC+ABS blend, low gloss and UV-stable, suitable for automotive interior applications. |
|||
Dart Drop, Total Energy | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® LG9000 PC+ABS (Asia Pacific) PC+ABS blend, low gloss and UV-stable, suitable for automotive interior applications. |
|||
Dart Drop, Total Energy | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® MC1300 PC+ABS Cycoloy MC1300 resin is an injection moldable PC/ABS blend with excellent flow and impact performance. It is designed for plating applications mostly used in the automotive industry. |
|||
Dart Drop, Total Energy | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® MC1300 PC+ABS (Asia Pacific) Cycoloy MC1300 resin is an injection moldable PC/ABS blend featuring excellent flow and impact performance. It is designed for plating applications mostly used in automotive industry. |
|||
Dart Drop, Total Energy | 40.0 J @Temperature -30.0 °C |
29.5 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C1110 PC+ABS High impact and ductility at 73F (23C) and -20F (-29C). |
|||
Dart Drop, Total Energy | 40.0 J @Temperature -30.0 °C |
29.5 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C1110 PC+ABS (Asia Pacific) High impact and ductility at 73F (23C) and -20F (-29C). |
|||
Dart Drop, Total Energy | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics GELOY XTPM405 ASA+PC High flow PC/ASA with improved impact at room and low temperatures. Improved release. Excellent weatherability for outdoor unpainted or clearcoated applications. Injection Moldable with large color .. |