Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 62.0 J @Temperature 23.0 °C |
45.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® EXL6414 PC PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
Dart Drop, Total Energy | 62.0 J @Temperature 23.0 °C |
45.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® EXL6414 PC (Asia Pacific) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
Dart Drop, Total Energy | 62.0 J @Thickness 3.20 mm, Temperature 0.000 °C |
45.7 ft-lb @Thickness 0.126 in, Temperature 32.0 °F |
Injection Molded, Total Energy; ASTM D3763 |
Styron EMERGEâ„¢ 9500CR Polycarbonate (PC) / Polyethylene Terephthalate (PET) Overview: EMERGEâ„¢ PC/PET 9500 CR advanced resin is a polycarbonate blend with excellent chemical resistance and ignition resistance properties. This grade was designed for use in medical equipm.. |
|||
Dart Drop, Total Energy | 62.0 J @Temperature 22.8 °C |
45.7 ft-lb @Temperature 73.0 °F |
ASTM D3763 |
Styron Pulse® 2000 ABS + PC Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Dart Drop, Total Energy | 62.0 J @Temperature -28.9 °C |
45.7 ft-lb @Temperature -20.0 °F |
ASTM D3763 |
Styron Pulse® 2100LG ABS + PC Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |