Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Gardner Impact = 31.6 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 31.6 J

@Temperature 23.0 °C
23.3 ft-lb

@Temperature 73.4 °F
ASTM D5420-96
LyondellBasell SEQUEL® E5000 TPO
Description: SEQUEL® E5000 thermoplastic olefinic elastomer (TPO) is designed for extrusion applications that require high mechanical stiffness, thermal stability, good low-temperature properties..