Mechanical Properties Metric English Comments
Flexural Modulus 0.00456 GPa

@Temperature 150 °C
0.661 ksi

@Temperature 302 °F
CW; ASTM D790
Haysite SDL® H261 Polyester, Static Dissipative
H261 is an advanced composite that combines high temperature resistant and high strength characteristics with static dissipative properties for use as wave and reflow solder pallets. SDL Grade H261..