Material Notes:
H261 is an advanced composite that combines high temperature resistant and high strength characteristics with static dissipative properties for use as wave and reflow solder pallets. SDL Grade H261 may be used as dedicated or adjustable flow solder carriers as well as surface mount pallets. Listed below are the expected performance properties of this material. H261 is available in sanded thicknesses from 3, 5, 6, 8, 10 and 12mm and in sheet sizes 36" x 72" and 48" x 96". Standard color is Black.Information provided by Haysite
Physical Properties Metric English Comments
Specific Gravity 1.83 g/cc
1.83 g/cc
ASTM D792
Water Absorption 0.16 %

@Time 86400 sec
0.16 %

@Time 24.0 hour
ASTM D651
Mechanical Properties Metric English Comments
Hardness, Barcol 48
48
ASTM D2583
Flexural Strength 41.73 MPa

@Temperature 150 °C
6053 psi

@Temperature 302 °F
LW; ASTM D790
44.73 MPa

@Temperature 150 °C
6487 psi

@Temperature 302 °F
CW; ASTM D790
186.76 MPa

@Temperature 25.0 °C
27087 psi

@Temperature 77.0 °F
LW; ASTM D790
228.02 MPa

@Temperature 25.0 °C
33071 psi

@Temperature 77.0 °F
CW; ASTM D790
Flexural Modulus 0.00406 GPa

@Temperature 150 °C
0.589 ksi

@Temperature 302 °F
LW; ASTM D790
0.00456 GPa

@Temperature 150 °C
0.661 ksi

@Temperature 302 °F
CW; ASTM D790
0.01043 GPa

@Temperature 25.0 °C
1.513 ksi

@Temperature 77.0 °F
LW; ASTM D790
0.01143 GPa

@Temperature 25.0 °C
1.658 ksi

@Temperature 77.0 °F
CW; ASTM D790
Thermal Properties Metric English Comments
CTE, linear 20.7 µm/m-°C
11.5 µin/in-°F
VSM 77110
Specific Heat Capacity 1.259 J/g-°C
0.3009 BTU/lb-°F
ASTM E-1269-05
Thermal Conductivity 0.425 W/m-K
2.95 BTU-in/hr-ft²-°F
ASTM E-1925-06
Electrical Properties Metric English Comments
Volume Resistivity 1e+05 - 1.00e+9 ohm-cm
1e+05 - 1.00e+9 ohm-cm
ASTM D257