Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0130 GPa @Temperature 23.0 °C |
1.89 ksi @Temperature 73.4 °F |
ASTM D790 |
ALM TPE-210-S Prototyping Polymer A thermoplastic elastomer used to produce parts with “rubber like” qualities. TPE 210-S exhibits good feature definition and infiltration with polyurethane will impart even higher toughness and ab.. |