Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.01143 GPa @Temperature 25.0 °C |
1.658 ksi @Temperature 77.0 °F |
CW; ASTM D790 |
Haysite SDL® H261 Polyester, Static Dissipative H261 is an advanced composite that combines high temperature resistant and high strength characteristics with static dissipative properties for use as wave and reflow solder pallets. SDL Grade H261.. |