Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.50 GPa @Temperature 23.0 °C |
218 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Crastin® ST820 BK503 PBT
(Unverified Data**) Crastin® ST820 BK503 is an unreinforced, Super Tough, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 1.50 GPa @Temperature 23.0 °C |
218 ksi @Temperature 73.4 °F |
50%RH; ASTM D790 |
DuPont Performance Polymers Zytel® 157HSL BK010 Nylon 612
(Unverified Data**) Zytel® 157HSL BK010 is a heat stabilized, weatherable, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 1.50 GPa @Temperature 23.0 °C |
218 ksi @Temperature 73.4 °F |
50%RH; ISO 178 |
DuPont Performance Polymers Zytel® 157HSL BK010 Nylon 612
(Unverified Data**) Zytel® 157HSL BK010 is a heat stabilized, weatherable, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 1.50 GPa @Temperature 80.0 °C |
218 ksi @Temperature 176 °F |
Practical Use (Water Absorption 2.7%); ASTM-D790 |
Toyobo GLAMIDE® TY-145TZ Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 1.50 GPa @Temperature 80.0 °C |
218 ksi @Temperature 176 °F |
Practical Use (Water Absorption 1.7%); ASTM-D790 |
Toyobo GLAMIDE® NB-5550 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 1.50 GPa @Temperature 23.0 °C |
218 ksi @Temperature 73.4 °F |
Practical Use; ASTM-D790 |
Toyobo GLAMIDE® T-779 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |