Mechanical Properties Metric English Comments
Flexural Modulus 3.45 GPa

@Temperature 23.0 °C
500 ksi

@Temperature 73.4 °F
DAM; ASTM D790
DuPont Performance Polymers Zytel® FR7025V0F NC010 Nylon 66  (Unverified Data**)
Zytel® FR7025V0F NC010 is a flame retardant polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuPont Performance..