Flexural Modulus 2.10 GPa

@Temperature 23.0 °C
305 ksi

@Temperature 73.4 °F
ISO 178
Polykemi AB POLYshine PBT D211 PBT, Modified
Information provided by Polykemi AB
Flexural Modulus 2.10 GPa

@Temperature 23.0 °C
305 ksi

@Temperature 73.4 °F
DAM; ISO 178
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612  (Unverified Data**)
Zytel® 151 NC010 is a PA 612 resin.Information provided by DuPont Performance Polymers
Flexural Modulus 2.10 GPa

@Temperature 260 °C
305 ksi

@Temperature 500 °F
ASTM D790
Saint-Gobain Meldin® 7211 CM Compression Molded Graphite and PTFE Filled Polyimide
Melidin® 7211 CM is a compression molded polyimide that contains 15% graphite and 10% PTFE fillers. This grade has the lowest coefficient of friction of the Meldin® 7000 series polyimides.Spe..
Flexural Modulus 2.10 GPa

@Temperature 80.0 °C
305 ksi

@Temperature 176 °F
Practical Use (Water Absorption 2.1%); ASTM-D790
Toyobo GLAMIDE® T-663G15 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 2.10 GPa

@Temperature 163 °C
305 ksi

@Temperature 325 °F
Wet (7 day immersion at 71°C)
Hexcel® HexPly® 954-3 Curing Cyanate Resin
HexPly® 954-3 is a 350°F (177°C) curing cyanate resin with excellent resistance to moisture absorption, outgassing and microcracking. HexPly® 954-3 is formulated for autoclave or press molding u..
Flexural Modulus 2.10 GPa

@Temperature 23.0 °C
305 ksi

@Temperature 73.4 °F
DAM; ISO 178
DuPont Performance Polymers Zytel® SC315 NC010 Nylon 612  (Unverified Data**)
Zytel® SC315 NC010 is an unreinforced, lubricated 612 polyamide suitable for injection molding. It has been developed for applications such as parts for the healthcare industry.Information provided..
Flexural Modulus 2.10 GPa

@Temperature 150 °C
305 ksi

@Temperature 302 °F
ASTM D790
DuPont Performance Polymers Rynite® 940 BK505 PET  (Unverified Data**)
Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers