Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.50 GPa @Temperature 23.9 °C |
653 ksi @Temperature 75.0 °F |
ASTM D790 |
Saint-Gobain Meldin® 7022 DF Direct Formed Graphite Filled Polyimide Melidin® 7022 DF is a direct formed polyimide that contains 40% graphite filler. This grade offers additional dimensional stability at elevated temperatures and the lowest CTE of any Meldin® .. |
|||
Flexural Modulus | 4.50 GPa @Temperature 80.0 °C |
653 ksi @Temperature 176 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-402 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 4.50 GPa @Temperature 80.0 °C |
653 ksi @Temperature 176 °F |
Practical Use (Water Absorption 2.0%); ASTM-D790 |
Toyobo GLAMIDE® T-403 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 4.50 GPa @Temperature -40.0 °C |
653 ksi @Temperature -40.0 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® TY-502NZ 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |