Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 46.9 GPa @Temperature 71.1 °C |
6800 ksi @Temperature 160 °F |
Wet; ASTM D790 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 3K PW Carbon Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Flexural Modulus | 46.9 GPa @Temperature 71.1 °C |
6800 ksi @Temperature 160 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 3K PW Carbon Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |