Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 5.82 J/cm @Thickness 12.7 mm |
10.9 ft-lb/in @Thickness 0.500 in |
LW, E-48/50 |
Industrial Laminates/Norplex NP180 Synthetic Fabric
(discontinued **) Description: aramid fabric material with a high performance epoxy resin matrix. Excellent electrical and mechanical properties at elevated temperatures and in adverse environments.Thickness Tested: .. |