Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.14 J/cm

@Thickness 12.7 mm
4.00 ft-lb/in

@Thickness 0.500 in
CW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP193E Synthetic Fabric
Description: 17 oz. aramid and "soft glass" fibers are combined to make a fabric that is stronger than pure aramid and less abrasive than glass fabrics. This material is impregnated with a high temp..