Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 19.8 J/cm @Thickness 12.7 mm |
37.0 ft-lb/in @Thickness 0.500 in |
CW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP555 Carbon Fiber
(discontinued **) Description: NP555 is composed of carbon fiber fabric and a phenolic resin system. It has excellent moisture resistance and physical properties. This material was designed to replace asbestos vane m.. |