Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.35 GPa @Thickness 3.20 mm |
1070 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID LW4403A(W) PA66+GF/MF40%, Low Warpage Feature: Injection Molding, PA66+GF/MF40%, Low WarpageApplication: Automotive (Timing Belt Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Modulus | 7.35 GPa @Thickness 3.20 mm |
1070 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOS GP2300 ABS+GF30%, General Purpose Feature: Injection Molding, ABS+GF30%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7, 9003-56-9 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ISO 178 |
Grupo Repol Dinalon® B1X25 G30V0 PA6 30% Glass Fiber, V0 Red Phosphorus and Halogen Free Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 230 DUS008 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fiber, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Flexural Modulus | 7.35 GPa @Thickness 3.20 mm |
1070 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUPOY GN2301F PC+GF30%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF30%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov.. |
|||
Flexural Modulus | 7.36 GPa | 1070 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM SF2260 PEI Blend (Asia Pacific) High flow Ultem for thin wall application |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DE0029 PC LNP* STAT-KON* DE0029 is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DE0029 PC (Asia Pacific) LNP* Stat-kon* DE0029 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® K4560 PBT (Europe-Africa-Middle East) 30% glass reinforced PBT. Impact modified, high flow, hydrolytically stable. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ISO 178 |
SABIC Innovative Plastics LNP Stat-kon PE002 PA 6 LNP* Stat-kon* PE002 is a compound based on Nylon 6 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americ.. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON REL42 PA 66 LNP* STAT-KON* REL42 is a compound based on Nylon 66 resin containing 20% PTFE, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON REL42 PA 66 (Asia Pacific) LNP* Stat-kon* REL42 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Flexural Modulus | 7.37 GPa | 1070 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DF006RXQ PC LNP* THERMOCOMP* DF006RXQ is a compound based on Polycarbonate resin containing 30% Glass Fiber. |
|||
Flexural Modulus | 7.35 GPa | 1070 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HM-3301GL PC, Glass Filled High Impact PC/GF material that is used for electric and electronic partsInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 7.37 GPa | 1070 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon DE002P PC (Asia Pacific) LNP STAT-KON* DE002P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the .. |
|||
Flexural Modulus | 7.38 GPa | 1070 ksi | ASTM D790 |
PlastxWorld CEVIAN® SUG30 ABS Glass fiber reinforced, high heat resistant and flame retarded ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by P.. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ASTM D790 |
Plenco 5482 Phenolic, Granular, Injection Molded PLENCO 05482 is an organic reinforced phenolic molding compound formulated with graphite to improve the abrasion resistance. 05482 is available in black and brown. 05482 is not recommended for elect.. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ASTM D790 |
Plenco 7500 Phenolic, Granular, Transfer Molded PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi.. |
|||
Flexural Modulus | 7.37 GPa | 1070 ksi | ISO 178-93 |
Wellman EcoLon® 2000-BK1 37% Post Consumer Compound Nylon 66 Description: Post Consumer Compound Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6600 GV 25 DCHP 25% Glass Fiber Nylon 66, Special Heat Ageing Stabilization, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ASTM D790, ISO 178 |
EPICHEM Epinyl PA 6 GF 30 ATP Polyamide 6, 30% Glass Characteristics: medium viscosity, 30% glass fibre, good toughness |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Polyamide 66 Zytel 80G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Inf.. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ISO 178 |
BASF Ultramid® B3ZG6 BK30564 30% Glass Filled PA6 (Dry) Ultramid B3ZG6 BK30564 is an impact-modified, pigmented black, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 114 Polypropylene, Glass Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ASTM D790 |
A. Schulman ComAlloy Voloy® 612 Nylon 6, Glass Fiber/Bead Reinforced, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Fiber/Bead Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | dry; ISO 178 |
DSM Stanyl® TQ261F5 PA46-GF25 25% Glass Reinforced, Heat Stabilized |
|||
Flexural Modulus | 7.35 GPa | 1070 ksi | ASTM D790 |
Gromax CCP PBT 5630-104C 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Flexural Modulus | 7.35 GPa @Thickness 3.20 mm |
1070 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID LW4009A(W) PA6+GF/MF40%, Low Warpage Feature: Injection Molding, PA6+GF/MF40%, Low WarpageApplication: Automotive (Timing Belt Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical |