Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.250 GPa | 36.3 ksi | ASTM D790-95 |
Multibase Multi-Pro® 2010 X Natural 20% Filler Content Polypropylene Data provided by Multibase. |
|||
Flexural Modulus | 0.250 GPa | 36.3 ksi | ASTM D790 |
NYCOA 2366 Plasticized Copolyamide TPE NYCOA 2366 is an extremely flexible and transparent Nylon copolymer specifically developed for extrusion applications such as high-end fishing line, and flexible tubing. NYCOA 2366 possesses an extr.. |
|||
Flexural Modulus | 0.250 GPa | 36.3 ksi | ASTM D790 |
Reliance Industries Reclair M26500 Polyethylene High flow Linear Low Density Polyethylene grade. Reclair M26500 is a butene comonomer with optimum levels of antioxidants.Characteristics:narrow molecular weight distribution, excellent processabi.. |
|||
Flexural Modulus | 0.250 GPa @Temperature 23.0 °C |
36.3 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET
(Unverified Data**) Hytrel® DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 49D and contains fine particle size carbon black.In.. |
|||
Flexural Modulus | 0.250 - 0.750 GPa | 36.3 - 109 ksi | ASTM D790 |
Micropol Microlink XL Crosslinkable Polyethylene Characteristics: exceptional toughness, exceptional enviromental stress cracking resistance, outstanding low temperature impact resistance down to -40°C, fully stabilized for outdoor use world wi.. |
|||
Flexural Modulus | 0.250 GPa | 36.3 ksi | ISO 178 |
Huntsman AVALON® 65 DB Thermoplastic Polyurethane Introduction: AVALON 65 DB is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 DB is part of the AVALON Perform Range and offers a premium soling material for sports foo.. |
|||
Flexural Modulus | 0.250 GPa | 36.3 ksi | ASTM D790 |
Sumitomo Chemical ESPOLEX® UT412A Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Flexural Modulus | 0.250 GPa | 36.3 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 105 Non-Reinforced, Injection Molding Grade Sodium Ionomer DescriptionFormion® FI 105 is a non-reinforced, transparent, injection molding grade Sodium Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and .. |
|||
Flexural Modulus | 0.250 GPa | 36.3 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 105 Non-Reinforced, Injection Molding Grade Sodium Ionomer DescriptionFormion® FI 105 is a non-reinforced, transparent, injection molding grade Sodium Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and .. |
|||
Flexural Modulus | 0.250 GPa | 36.3 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 105 Non-Reinforced, Injection Molding Grade Sodium Ionomer DescriptionFormion® FI 105 is a non-reinforced, transparent, injection molding grade Sodium Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and .. |
|||
Flexural Modulus | 0.250 GPa | 36.3 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 105 Non-Reinforced, Injection Molding Grade Sodium Ionomer DescriptionFormion® FI 105 is a non-reinforced, transparent, injection molding grade Sodium Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and .. |
|||
Flexural Modulus | 0.250 GPa | 36.3 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 105 Non-Reinforced, Injection Molding Grade Sodium Ionomer DescriptionFormion® FI 105 is a non-reinforced, transparent, injection molding grade Sodium Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and .. |
|||
Flexural Modulus | 0.250 GPa | 36.3 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 105 Non-Reinforced, Injection Molding Grade Sodium Ionomer DescriptionFormion® FI 105 is a non-reinforced, transparent, injection molding grade Sodium Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and .. |
|||
Flexural Modulus | 0.250 GPa | 36.3 ksi | ASTM D790 |
DuPont™ Surlyn® 9720 Ionomer Resin, Zinc Surlyn® 9720 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Flexural Modulus | 0.250 GPa | 36.3 ksi | ASTM D790 |
DuPont™ Surlyn® 9721 Ionomer Resin, Zinc Surlyn® 9721 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Flexural Modulus | 0.250 GPa | 36.3 ksi | ASTM D790 |
DuPont™ Surlyn® 9950 Ionomer Resin, Zinc Surlyn® 9950 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Flexural Modulus | 0.250 GPa | 36.3 ksi | SAE J949 |
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (9 mm Molded Thickness) AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 0.250 GPa | 36.3 ksi | SAE J949 |
Azdel SuperLite® SL551800-100 PP Resin Matrix / 55% Glass Fiber (10 mm Molded Thickness) AZDEL SuperLite® SL551800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 0.250 GPa | 36.3 ksi | ASTM D790 |
C.O.I.M. LARIPUR® LPR6260 PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Flexural Modulus | 0.250 GPa | 36.3 ksi | ISO 178 |
Borealis LE6022 Polyethylene Modified Jacketing Compound LE6022 is a black low density copolymer modified polyethylene compound. It is characterized by excellent crack resistance and mechanical properties and low temperature performance in combination wit.. |
|||
Flexural Modulus | 0.250 GPa | 36.3 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 75HF Nylon 66/6, Heat Stabilized, Conditioned Vydyne® 75HF is a medium-high-viscosity, heat-stabilized PA66/6 copolymer resin designed for extrusion applications. It is available in natural color only. Vydyne 75HF resin offers a well-balanced .. |