Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.012589 GPa | 1.8259 ksi | ASTM D790 |
Sekisui PIOCELAN OP-30DB Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |