Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0430 GPa @Thickness 2.00 mm |
6.24 ksi @Thickness 0.0787 in |
molded plaque, cured 20 hr at 100°C; ASTM D790 |
BASF Elastollan® 1185A10W Wire & Cable Grade Polyurethane Elastomer As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Flexural Modulus | 0.0430 GPa @Thickness 2.00 mm |
6.24 ksi @Thickness 0.0787 in |
molded plaque, cured 20 hr at 100°C; ASTM D790 |
BASF Elastollan® 1185A10X Wire & Cable Grade Polyurethane Elastomer Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Flexural Modulus | 0.0430 GPa @Thickness 2.00 mm |
6.24 ksi @Thickness 0.0787 in |
molded plaque, cured 20 hr at 100°C; ASTM D790 |
BASF Elastollan® 1185A10U Wire & Cable Grade Polyurethane Elastomer As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Flexural Modulus | 0.0430 GPa @Thickness 2.00 mm |
6.24 ksi @Thickness 0.0787 in |
molded plaque, cured 20 hr at 100°C; ASTM D790 |
BASF Elastollan® 1185A10V Wire & Cable Grade Polyurethane Elastomer Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Flexural Modulus | 0.0430 GPa @Thickness 2.00 mm |
6.24 ksi @Thickness 0.0787 in |
molded plaque, cured 20 hr at 100°C; ASTM D790 |
BASF Elastollan® 1185A10Y Wire & Cable Grade Polyurethane Elastomer Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |