Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 6.24 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.0430 GPa

@Thickness 2.00 mm
6.24 ksi

@Thickness 0.0787 in
molded plaque, cured 20 hr at 100°C; ASTM D790
BASF Elastollan® 1185A10W Wire & Cable Grade Polyurethane Elastomer
As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.
Flexural Modulus 0.0430 GPa

@Thickness 2.00 mm
6.24 ksi

@Thickness 0.0787 in
molded plaque, cured 20 hr at 100°C; ASTM D790
BASF Elastollan® 1185A10X Wire & Cable Grade Polyurethane Elastomer
Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.
Flexural Modulus 0.0430 GPa

@Thickness 2.00 mm
6.24 ksi

@Thickness 0.0787 in
molded plaque, cured 20 hr at 100°C; ASTM D790
BASF Elastollan® 1185A10U Wire & Cable Grade Polyurethane Elastomer
As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.
Flexural Modulus 0.0430 GPa

@Thickness 2.00 mm
6.24 ksi

@Thickness 0.0787 in
molded plaque, cured 20 hr at 100°C; ASTM D790
BASF Elastollan® 1185A10V Wire & Cable Grade Polyurethane Elastomer
Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.
Flexural Modulus 0.0430 GPa

@Thickness 2.00 mm
6.24 ksi

@Thickness 0.0787 in
molded plaque, cured 20 hr at 100°C; ASTM D790
BASF Elastollan® 1185A10Y Wire & Cable Grade Polyurethane Elastomer
Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.