Mechanical Properties Metric English Comments
Flexural Modulus 0.0972 GPa
14.1 ksi
ASTM D790
Lubrizol ESTANE® 58215 Ether Based Thermoplastic Polyurethane
Features: Excellent physical properties, hydrolysis resistance and improved temperature resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and b..