Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.117 GPa | 17.0 ksi | method 1, Proc.B; ASTM D-790 |
Multibase Multi-Flex® TPE A 9002-SR BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Flexural Modulus | 0.117 GPa | 16.9 ksi | ASTM D790 |
SK Chemicals SKYPEL P147D Productivity Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Flexural Modulus | 0.117 GPa | 17.0 ksi | 2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 A |
Dow FLEXOMER™ DFDB-9042 NT Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ DFDB-9042 NT is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It has value as a sealant layer in multilayer film structures for dry and liquid packaging. I.. |