Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.124 GPa | 18.0 ksi | 3 pt. secant; ASTM D790 |
Chevron Phillips 1008.5 Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; ASTM D 4976 Classification: PE 112, A 14200Characteristics: Excellent Flexibility, Excellent Flow, Good Warping Resistance, Moderate Mold Release, Moderate ESCRApplications:.. |
|||
Flexural Modulus | 0.124 GPa | 18.0 ksi | 1% Secant; ASTM D790 |
Plastics Group Polifil® RP-LDPE Low Density Polyethylene Polifil® RP-Low Density Polyethylene is a soft, tough material with good clarity and high chemical resistance. LDPE remains flexible and retains impact strength at very low temperatures. High melt .. |
|||
Flexural Modulus | 0.124 GPa | 18.0 ksi | 3 pt. secant; ASTM D790 |
Chevron Phillips Marlex® 1007 Injection Molding Resin Resin Type: Homopolymer; ASTM D 4976 Classification: PE 113, A 25200Characteristics: Excellent Flexibility, Good Flow, Good Warping Resistance, Moderate Mold Release, Good ESCRApplications:Houseware.. |