Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 0.130 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.130 GPa
18.9 ksi
ISO 178
Polimeri Europa Riblene® MM 20 Low Density Polyethylene - Injection Molding
Riblene MM 20 is a medium fluidity low density polyethylene resin (LDPE).Parts made by Riblene MM 20 are characterized by a high flexibility.Main Applications: Riblene MM 20 is suitable for injecti..
Flexural Modulus 0.130 GPa
18.9 ksi
ISO 178
Polimeri Europa Riblene® MM 20 R Low Density Polyethylene - Injection Molding
Riblene MM 20 R is a medium fluidity low density polyethylene resin (LDPE).Parts made by Riblene MM 20 R are characterized by a high flexibility.Main Applications: Riblene MM 20 R is suitable for i..
Flexural Modulus 0.130 GPa
18.9 ksi
ISO 178
Polimeri Europa Riblene® MP 20 Low Density Polyethylene - Injection Molding
Riblene MP 20 is a medium fluidity low density polyethylene resin (LDPE).Parts made by Riblene MP 20 are characterized by a high flexibility.Main Applications: Riblene MP 20 is suitable for injecti..
Flexural Modulus 0.130 GPa
18.9 ksi
ASTM D790
Rotuba H2 Cellulose Acetate
Property values at 50% RH.Data provided by the manufacturer.
Flexural Modulus 0.130 GPa
18.9 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCD801AU PPE-TPE (Asia Pacific)
Flexible, UV stabilized, halogen free extrusion grade for applications such as wire insulation and cable jacket. Good color stability after UV weathering per ASTM D4459. Light color capable. Flame r..
Flexural Modulus 0.130 GPa
18.9 ksi
12.5 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCD933 PPE-TPE
Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as insulation of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN..
Flexural Modulus 0.130 GPa
18.9 ksi
12.5 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCD933 PPE-TPE (Asia Pacific)
Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as insulation of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN..
Flexural Modulus 0.130 GPa
18.9 ksi
12.5 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCP821 PPE-TPE
Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain ..
Flexural Modulus 0.130 GPa
18.9 ksi
12.5 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCP821 PPE-TPE (Asia Pacific)
Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain ..
Flexural Modulus 0.130 GPa
18.9 ksi
12.5 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCP821 PPE-TPE (Europe-Africa-Middle East)
Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain ..
Flexural Modulus 0.130 GPa
18.9 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCP821U PPE-TPE (Asia Pacific)
UV stabilized, halogen free Flexible Noryl injection molding grade for overmolding applications such as plugs, strain relief's, and connectors. Good color stability after UV weathering per ASTM D445..
Flexural Modulus 0.130 GPa
18.9 ksi
12.5 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCD933 PPE-TPE (Europe-Africa-Middle East)
Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as insulation of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN..
Flexural Modulus 0.130 GPa
18.9 ksi
ASTM D638
Arkema Group LOTADER® TX 8030 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER TX 8030 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure autoclave process. LOTADER TX 8030 is an adhesive designed for extrusion coating ..
Flexural Modulus 0.130 GPa
18.9 ksi
ASTM D790
LATI LATISTAT 48/9900-03 Ethylene Vinyl Acetate (EVA) Base Conductive Plastic  (Unverified Data**)
Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable..
Copyright © lookpolymers.com All Rights Reserved