Mechanical Properties Metric English Comments
Flexural Modulus 0.160 GPa
23.2 ksi
STN EN ISO 178
Plastcom PLASTALEN® TPU N 85 LTS TPU
Modified TPU. Use in all industry sectors. Delivered in the black.Information Provided by Plastcom spol. s r.o.
Flexural Modulus 0.160 GPa
23.2 ksi
ASTM D790
Rotuba H5 Cellulose Acetate
Property values at 50% RH.Data provided by the manufacturer.
Flexural Modulus 0.160 GPa
23.2 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCD891B PPE-TPE (Asia Pacific)
Non-halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications. Strong flame retardant performance capable of meeting VW-1 and 80°C end use tempera..
Flexural Modulus 0.160 GPa
23.2 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCD891B PPE-TPE (Europe-Africa-Middle East)
Non-halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications. Strong flame retardant performance capable of meeting VW-1 and 80°C end use tempera..
Flexural Modulus 0.160 GPa
23.2 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCD933 PPE-TPE
Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as insulation of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN..
Flexural Modulus 0.160 GPa
23.2 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCD933 PPE-TPE (Asia Pacific)
Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as insulation of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN..
Flexural Modulus 0.160 GPa
23.2 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCD891B PPE-TPE
Non-halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications. Strong flame retardant performance capable of meeting VW-1 and 80°C end use tempera..
Flexural Modulus 0.160 GPa
23.2 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCD933 PPE-TPE (Europe-Africa-Middle East)
Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as insulation of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN..
Flexural Modulus 0.160 GPa
23.2 ksi
ASTM D790
Arkema Group Pebax® 5533 Polyether Block Amide (PEBA)
Information provided by Arkema Group
Flexural Modulus 0.160 GPa
23.2 ksi
Conditioned 15 days at 23°C - 50% RH; ISO178
Arkema Group Pebax® Rnew 55R53 SP 01 Polyether Block Amide (PEBA)
Polyether block amide Pebax® 55R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV..
Flexural Modulus 0.160 GPa

@Temperature 93.0 °C
23.2 ksi

@Temperature 199 °F
ASTM Test
BASF Ultramid® 8255 HS PA6 (Dry)
Ultramid 8255 HS is a heat stabilized, impact modified type 6 nylon graft copolymer developed for both injection molding and extrusion applications. It exhibits varying levels of toughness and fle..
Flexural Modulus 0.160 GPa
23.2 ksi
ASTM D790
ExxonMobil Iotek® 7310 Zinc Ionomer  (discontinued **)