ExxonMobil Iotek® 7310 Zinc Ionomer  (discontinued **)

Category Polymer , Thermoplastic , Ionomer , Ionomer, Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Iotek® 7310 Zinc Ionomer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.A low melt index zinc ionomer made from an ethylene acrylic acid base polymer.Applications: Injection molding; Impact modifier of polyamide.
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
Exxon Method
Melt Flow 1.0 g/10 min
1.0 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Hardness, Shore D 52
52
ASTM D2240
Tensile Strength, Ultimate 24.0 MPa
3480 psi
ASTM D638
Elongation at Break 520 %
520 %
ASTM D638
Flexural Modulus 0.160 GPa
23.2 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 64.0 °C
147 °F
Exxon Method
Vicat Softening Point 69.0 °C
156 °F
Rate B; ASTM D-1525