Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.275 - 0.700 GPa | 39.9 - 102 ksi | Average value: 0.504 GPa Grade Count:15 |
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum.. |
|||
Flexural Modulus | 0.275 GPa @Temperature 120 °C |
39.9 ksi @Temperature 248 °F |
ASTM D790 |
LATI LATILUB 82-01M Nylon 12 Base, 1% Molybdenum Disulfide Self Lubricating Plastic
(discontinued **) Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Flexural Modulus | 0.275 - 0.685 GPa @Temperature 60.0 - 120 °C |
39.9 - 99.4 ksi @Temperature 140 - 248 °F |
Average value: 0.450 GPa Grade Count:1 |
Overview of materials for Nylon 12 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en.. |
|||
Flexural Modulus | 0.275 - 0.700 GPa | 39.9 - 102 ksi | ASTM D790 |
Zeus PTFE Tubing Zeus offers a wide range of standard size products and precision custom PTFE Tubing. PTFE Tubing has become the gold standard in industries requiring the ultimate in lubricity, high temperature use,.. |