Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 0.350 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus >= 0.350 GPa
>= 50.8 ksi
ASTM D790
NIZHNEKAMSKNEFTEKHIM PE 4222M (224F7) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Flexural Modulus 0.350 GPa

@Temperature 93.0 °C
50.8 ksi

@Temperature 199 °F
ASTM D790
BASF Capron® 8200 NL Nylon 6 (DAM)  (discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Flexural Modulus 0.350 GPa

@Temperature 93.0 °C
50.8 ksi

@Temperature 199 °F
ASTM D790
BASF Capron® 8202 NL Nylon 6 (DAM)  (discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Flexural Modulus 0.350 GPa
50.8 ksi
cond., 2 mm/min; ISO 178-A
Lanxess Durethan® BC 600 HTS DUSXBL 900116 Nylon 6, Impact Modified
PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Flexural Modulus 0.350 GPa
50.8 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP TX97446 PU
LNP* LUBRICOMP* TX97446 is a compound based on Polyurethane containing Proprietary Fillers. Added feature of this material is: Wear Resistant.
Flexural Modulus 0.350 GPa
50.8 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Stat-kon TD000
LNP* Stat-kon* TD000 is a compound based on Polyurethane resin. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 0.350 GPa
50.8 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON TD000 PU
LNP* STAT-KON* TD000 is an unfilled compound based on Polyurethane resin. Added feature of this material is: Electrically Conductive.
Flexural Modulus 0.350 GPa
50.8 ksi
ISO 178-1975
SIDPEC EGYPTENE® LL 0550 AA LLDPE Injection Molding
Applications:House waresVery thin-walled food containersLidsInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products
Flexural Modulus 0.350 GPa
50.8 ksi
ASTM D790
Sumitomo Chemical ESPOLEX® 907 Thermoplastic Elastomer
ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi..
Flexural Modulus 0.350 GPa
50.8 ksi
DIN EN ISO 178
Wolf Kunststoff ZEDEX® ZX-100EL55 A1F Polymer Alloy, Elastomer Modified
Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol..
Flexural Modulus 0.350 GPa
50.8 ksi
ISO 178
Polyram PlusTek PD120BK11 Nylon 12 for Extrusion, UV Stabilized
Nylon 12 UV stabilized for extrusion application.Information provided by Polyram.
Flexural Modulus 0.350 GPa
50.8 ksi
ISO 178
Chengdu Polyster CH7563 Thermoplastic Polyether-ester Elastomer (TPEE)
Poly-basic block copolymer. Good compatibility with PBT, PET and PA. For blending with PBT, PET and PA to improve impact resilience properties.Information provided by Chengdu Polyster Co., Ltd.
Flexural Modulus 0.350 GPa
50.8 ksi
ASTM D790
Covestro Bayflex® XGT-50 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of..
Flexural Modulus 0.350 GPa
50.8 ksi
ASTM D790
DuPont™ Surlyn® 8920 Ionomer Resin, Sodium
Surlyn® 8920 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu..
Flexural Modulus 0.350 GPa
50.8 ksi
ASTM D790
DuPont™ Surlyn® 8940 Ionomer Resin, Sodium
Surlyn® 8940 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu..
Flexural Modulus 0.350 GPa
50.8 ksi
ASTM D790
DuPont™ Surlyn® PC100 Ionomer Resin, Highest Clarity, Sodium
Surlyn® PC100 luxury molding resin is a "select" grade of Surlyn® 8920, controlled to achieve the highest possible optical clarity in molded perfume jars and caps. It complies with the provisions ..
Flexural Modulus 0.350 GPa
50.8 ksi
ISO 178
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET+PBT  (Unverified Data**)
Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsHytrel DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Depl..
Flexural Modulus 0.350 GPa
50.8 ksi
ASTM D790
C.O.I.M. LARIPUR® LPR6325 Special Adipate Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
Flexural Modulus 0.350 GPa

@Temperature 93.0 °C
50.8 ksi

@Temperature 199 °F
ASTM Test
BASF Ultramid® 8202 HS PA6 (Dry)
Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab..
Flexural Modulus 0.350 GPa

@Temperature 93.0 °C
50.8 ksi

@Temperature 199 °F
ASTM Test
BASF Ultramid® 8202 PA6 (Dry)
Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult..
Flexural Modulus 0.350 GPa
50.8 ksi
SAE J949
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (8 mm Molded Thickness)
AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Copyright © lookpolymers.com All Rights Reserved