Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.370 GPa | 53.7 ksi | ISO 178 |
FKuR Kunststoff Bio-Flex® F 1130 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Flexural Modulus | 0.370 GPa | 53.7 ksi | at RT method 1, proc. B; ASTM D-790 |
Multibase Multi-Flex® TPE A 5009 Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Flexural Modulus | 0.370 GPa | 53.7 ksi | ASTM D790 |
Lubrizol ESTANE® 58237 Ether Based Thermoplastic Polyurethane Features: High moisture vapor transmission. Good physical properties and elasticity.Uses: Blown and flat die/cast film extrusion.Available in Americas, Europe, Middle East, Africa, India and AsiaInf.. |
|||
Flexural Modulus | 0.370 - 0.560 GPa @Temperature 60.0 - 90.0 °C |
53.7 - 81.2 ksi @Temperature 140 - 194 °F |
Average value: 0.465 GPa Grade Count:1 |
Overview of materials for Polypropylene Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp.. |