Mechanical Properties Metric English Comments
Flexural Modulus 0.380 GPa
55.1 ksi
ASTM D790
ICO Polymers ICORENEâ„¢ 110-1329 LMDPE Rotational Molding Resin
Description: ICORENE 110-1329 is a linear medium density polyethylene developed for use in rotational molding. This is a very fast processing material that quickly molds out to offer low surface po..
Flexural Modulus 0.380 GPa
55.1 ksi
1.3 mm/min; ASTM D790
ICO Polymers ICORENEâ„¢ 115-1329 LMDPE Rotational Molding Resin
Description: ICORENE 115-1329 is a linear medium density polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and gene..
Flexural Modulus 0.380 GPa
55.1 ksi
1.33 mm/min; ASTM D790
ICO Polymers ICORENEâ„¢ 190-1329 LMDPE Rotational Molding Resin
Description: ICORENE 190-1329 is a compounded linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and sti..
Flexural Modulus 0.380 GPa
55.1 ksi
ISO 178
Solvay TECHNYL® C 442 Black V PA6, Conditioned
Description: Unreinforced polyamide PA6, high viscosity, with high flexibility and very high impact resistance even at low temperature, for extrusion.Available in: Europe Product Applications: It ha..
Flexural Modulus 0.380 GPa
55.1 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP TX97446 PU
LNP* LUBRICOMP* TX97446 is a compound based on Polyurethane containing Proprietary Fillers. Added feature of this material is: Wear Resistant.
Flexural Modulus 0.380 GPa
55.1 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics ULTEM STM1500 PEI Copolymer
Siloxane polyetherimide block copolymer. Wire and cable use. Strength and flexibility.
Flexural Modulus 0.380 GPa
55.1 ksi
cond; ISO 178
DSM Novamid® ST145 NAT PA6-I
Impact Modified, Injection Molding
Flexural Modulus 0.380 GPa
55.1 ksi
Dow DOWLEX™ 2500 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2500 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and tear strength with high impact strength. It..
Flexural Modulus 0.380 GPa
55.1 ksi
ASTM D790
C.O.I.M. LARIPUR® LPR6650 Modified Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
Flexural Modulus 0.380 GPa
55.1 ksi
ASTM D790
Ashley Polymers Ashlene® 940H Nylon 11
A general purpose highly flexible natural Nylon 11 resin with UV stabilizers.Data provided by the manufacturer
Flexural Modulus 0.380 GPa
55.1 ksi
ASTM D790
Ashley Polymers Ashlene® D930H Nylon 12
A plasticized Nylon 12 offering improved flexibility with superior moisture and chemical resistance. Also UV and heat stabilized, available in natural and precolored. Any color other than natural ..
Flexural Modulus 0.380 GPa
55.1 ksi
ASTM D790
Ashley Polymers Ashlene® T940H Nylon 11
A general purpose, highly flexible Natural Nylon 11 resin with UV stabilizers.Data provided by the manufacturer
Flexural Modulus 0.380 - 1.38 GPa
55.1 - 200 ksi
Average value: 0.985 GPa Grade Count:11
Overview of materials for Nylon 11, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Flexural Modulus 0.380 - 32.6 GPa
55.1 - 4730 ksi
Average value: 6.74 GPa Grade Count:797
Overview of materials for Polyetherimide (PEI)
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat..