Mechanical Properties Metric English Comments
Flexural Modulus 0.420 GPa
60.9 ksi
1.3 mm/min; ASTM D790
ICO Polymers ICORENEâ„¢ 110-1328 LMDPE Rotational Molding Resin
Description: ICORENE 110-1328 is a linear medium density polyethylene developed for use in rotational molding. This is a very fast processing material that quickly molds out to offer low surface po..
Flexural Modulus 0.420 GPa
60.9 ksi
1.3 mm/min; ASTM D790
ICO Polymers ICORENEâ„¢ 115-1323 LMDPE Rotational Molding Resin
Description: ICORENE 115-1323 is a linear medium density polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and gene..
Flexural Modulus 0.420 GPa
60.9 ksi
1.3 mm/min; ASTM D790
ICO Polymers ICORENEâ„¢ 190-1323 LMDPE Rotational Molding Resin
Description: ICORENE 190-1323 is a linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and stiffness. Key..
Flexural Modulus 0.420 GPa
60.9 ksi
1.3 mm/min; ASTM D790
ICO Polymers ICORENEâ„¢ 190-1328 LMDPE Rotational Molding Resin
Description: ICORENE 190-1328 is a linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and stiffness. Key..
Flexural Modulus 0.420 GPa
60.9 ksi
1.3 mm/min; ASTM D790
ICO Polymers ICORENEâ„¢ 324-1323 LMDPE Rotational Molding Resin
Description: ICORENE 324-1323 is a linear medium density polyethylene developed for use in rotational molding. It has very good flow properties allowing the material to reproduce fine detail and me..
Flexural Modulus 0.420 GPa
60.9 ksi
ASTM D790
Sumitomo Chemical ESPOLEX® WT521 Thermoplastic Elastomer
ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi..
Flexural Modulus 0.420 GPa
60.9 ksi
SAE J949
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness)
AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Modulus 0.420 GPa
60.9 ksi
ASTM D790
DuPont™ Surlyn® 7940 Ionomer Resin, Lithium
Surlyn® 7940 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with lithium ions. The amount of MAA and ne..