Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.310 - 0.483 GPa | 45.0 - 70.0 ksi | ASTM D790 |
Buckeye Polymers BP FLEX D4107 CU BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |