Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
Owens Corning Glass Fiber Reinforced Polyurethane, Milled Fibers (RRIM), 13 wt.% glass Polyurethane is normally used for its structural properties when molded. It is highly resistant to most organic solvents. It is not recommended for use with strong acids and alkalis, steam, fuels, a.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | at 1%; ASTM D790 |
NOVA Chemicals Novapol® LA-0224-A LDPE Foam Resin Excellent stiffness, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blown film.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
NOVA Chemicals Sclair® 31E LLDPE Extrusion Resin Features: Excellent tensile properties, excellent impact toughness, outstanding gloss and clarity, excellent processability.Applications: Coating and sheathing.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
M. Holland Company LL508 LLDPE
(discontinued **) Features: High ESCR (Stress Crack Resist.), Good Flexibility, High FlowUses: Closures, Household GoodsApprovals: FDA 21 CFR 177.1520(c) 3.1bProcessing Method: Injection MoldingInformation provided b.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
Eastman 1924P Polyethylene
(discontinued **) Low-density polyethylene 1924P is a resin in the boardstock coating industry for use in breadboard, cupstock, and liquid packaging board. This material has an excellent combination of low neck-in, .. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790M |
DSM Somos® 8110 Epoxy Photopolymer
(discontinued **) DescriptionDSM Somos® 8110 is a high-speed liquid photopolymer that produces flexible, high-impact-strength, accurate parts using stereolithography machines. It has a wide processing latitude and .. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
Multibase Multi-Flex® A 8832 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Thermal Stability, GoodOzone Resistant Noise Damping Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsInformation provided by Mult.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 504 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an extrusion grade olefinic thermoplastic elastomer suitable for profile extrusion or blow molding. Characteristics of this product include excellent low temperature.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | 1% secant - transverse direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | transverse direction; ASTM D882 |
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 504 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an extrusion grade olefinic thermoplastic elastomer suitable for profile extrusion or blow molding. Characteristics of this product include excellent low temperature.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | 1% secant - transverse direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | 1% secant - transverse direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 504 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | 1% secant - transverse direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | 1% secant - transverse direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | transverse direction; ASTM D882 |
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | 1% secant - transverse direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an extrusion grade olefinic thermoplastic elastomer suitable for profile extrusion or blow molding. Characteristics of this product include excellent low temperature.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an extrusion grade olefinic thermoplastic elastomer suitable for profile extrusion or blow molding. Characteristics of this product include excellent low temperature.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
Covestro Baydur® 646 Polyurethane Structural Foam RIM, Density 20 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | Compression molded parts prepared according to ASTM D 1928, method 1, procedure B.; ASTM D790 |
Dow DNDB-7441 NT 7 Linear Low Density Polyethylene Resin DOW DNDB-7441 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in hose and tube applications. It also has utility in gasketing, spiral wound hose, and corrugated hose .. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | |
BASF Ultramid® 8270 HS PA6 (Dry) Ultramid 8270 HS is a thermally modified PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile extrusion, and other applications requi.. |
|||
Flexural Modulus | 0.310 - 0.483 GPa | 45.0 - 70.0 ksi | ASTM D790 |
Buckeye Polymers BP FLEX D4107 CU BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 504 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 504 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an extrusion grade olefinic thermoplastic elastomer suitable for profile extrusion or blow molding. Characteristics of this product include excellent low temperature.. |