Polymer Property : Flexural Modulus = 0.616 GPa
Polymer Property :
Flexural Modulus =
0.616 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Modulus
0.616
GPa
89.3
ksi
Secant 1%; ASTM D-790-95
Multibase Multi-Flex® TPO D 5302 Q
Data provided by Multibase.