Multibase Multi-Flex® TPO D 5302 Q

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Multibase
Trade Name Multi-Flex® TPO
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPO D 5302 Q.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.8995 g/cc
0.03250 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.011 cm/cm
0.011 in/in
ASTM D955-89
Melt Flow 0.95 g/10 min
0.95 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate 26.3 MPa
3810 psi
ASTM D638-95
Elongation at Break 593 %
593 %
ASTM D638-95
Flexural Modulus 0.616 GPa
89.3 ksi
Secant 1%; ASTM D-790-95
Tear Strength 159 kN/m
907 pli
ASTM D624-95